Black castings in jewellery, figurines and decorative parts fail for three reasons: exotherm, trapped air and early demould. A practical note on all three.

Deep black epoxy jewellery and decorative casting workshop with polished black parts, realistic industrial photography

Decorative and jewellery casting in black epoxy is a small-volume, high-visibility application. A 30 mm figurine with a bubble at the shoulder or a soft centre is a reject, and both faults trace back to the same two variables: how much heat the mass generates, and how much air it holds.

What Thick Means for a Filled System

A black paste at 15 percent reduces the reactive mass per unit volume and slows heat build-up, which is why filled systems can be poured thicker than neat resin without cracking. The same dilution slows the core, and the surface can reach demould hardness while the centre is still soft.

SEP-988 deep black epoxy cast cat figurine and glossy black epoxy parts
Deep black cast parts in epoxy, including a cat figurine and machined components

Exotherm and the 500 g Reference Mass

Mass at 25 °CPeak exotherm, 15% SEP-988Peak exotherm, unfilled
100 g45–65 °C100–130 °C
500 g60–90 °C140–180 °C
2 kg95–125 °C180–210 °C

For a decorative part the limit is not the resin but the mould and the insert. Silicone moulds insulate, so a 2 kg casting in a thick silicone block runs hotter than the same mass in an open frame. Measure the first article with a thermocouple rather than estimating from the datasheet.

Bubbles: Source, Not Symptom

Bubbles in a black casting come from four places, and only one of them is the resin.

  • Air entrained during mixing, visible as a foam layer on the surface of the mixed mass.
  • Air trapped against the mould wall when the pour front folds over.
  • Moisture on a filler or an insert, which expands as the mass heats.
  • Shrinkage voids in the thermal centre of a thick section, which look like bubbles but form after gel.
SEP-988 high gloss jet black epoxy bear figurine bangle and round casting
Polished jet black epoxy castings, including a bear figurine and a bangle

Mixing under vacuum removes the first. A slow, single-point pour from the deepest corner removes most of the second. Drying fillers and inserts removes the third. Only the fourth is a section-design problem, and it is solved by feeding the mould or by casting in two stages.

Demould Timing

Demould when the section, not the surface, has reached hardness. In a 20 mm black casting at 25 °C that is typically 12 to 18 hours with SEP-988 at 15 percent, against 6 to 10 hours for the same resin unfilled.

SEP-988 deep black epoxy dome and disc castings under daylight
Deep black epoxy dome and disc castings inspected under daylight

Pulling early is the most common cause of a surface that looks perfect and a part that deforms a week later. If the schedule has to be shortened, raise the mould temperature rather than shortening the demould time, and verify the core hardness on a sacrificial part.

Related Reading

See the control module potting note for gel time and void control. Grade data is listed separately on the SEP-988 page.