Technical Articles2026-11-26

SEP-955 Dioxazine Violet Casting for Artware, River Tables and Decorative Epoxy

SEP-955 in decorative epoxy casting: 3 to 8 phr dosage, transparency versus depth, artware and river table practice, staged pours and finishing for violet castings.

Two glossy violet epoxy paw castings made with SEP-955

SEP-955 suits decorative epoxy casting because 15 percent Pigment Violet 23 in an epoxy carrier disperses into the pour without adding solvent, and a 3 to 8 phr addition gives a violet that reads translucent at thin edges and close to opaque in a thick body. It is a colour product: exotherm, bubble release and cure depth still come from the resin, hardener and pour plan.

Why dioxazine violet works in clear castings

PropertySEP-955
PigmentC.I. Pigment Violet 23, CAS 215247-95-3
Pigment content15% by weight
CarrierDGEBA epoxy resin with reactive diluent
Fineness of grind3–5 μm
Density at 25 °C1.17 g/mL
Heat resistance of cured film250 °C
Light fastnessGrade 7–8
Standard packaging20 kg net plastic pail

Dioxazine violet has strong tinting strength and a reddish cast that reads warm under tungsten light and cooler in daylight. In a clear casting that character is an advantage: less paste is needed to reach a deep shade, and the colour survives polishing because the pigment is dispersed through the cured body rather than sitting on the surface.

Artware and small castings

Small moulded pieces concentrate attention on saturation and surface. At 3 to 5 phr SEP-955 gives a solid violet; at 6 to 8 phr the colour becomes deep and the piece reads darker at the core than at the skin. Curved shapes create real differences in section thickness, so the same mix looks lighter on thin petals and deeper in the mass behind them.

Violet rose casting made with SEP-955
Violet rose casting made with SEP-955. Curved petals create thin and thick sections in the same piece, so the violet reads lighter at the edges and deeper in the body.

Small parts also cure quickly relative to their mass, which limits exotherm but leaves less time for bubbles to rise. Warm the resin and paste to a controlled 20 to 25 °C, mix gently, and vacuum de-gas before pouring if the mould cannot be pressure-cast.

River tables and deep pours

A river table is a thick, often wide pour between two slabs, and the colour has to stay consistent across a large volume. At 2 to 6 phr the violet keeps some translucency, which lets light move through the river and keeps the wood-to-resin boundary readable. Depth changes everything. A 40 mm river section holds heat longer than a 10 mm coaster, and the violet will not show you that the centre is overheating. Plan the pour in stages, follow the resin supplier's maximum pour depth, and treat colour as the last variable to adjust. Exotherm control for large masses is covered in violet potting, encapsulation and epoxy adhesives.

Decorative objects, plaques and polished pieces

Plaques, signage blanks and desk objects often combine flat surfaces with recessed detail. Recessed lettering traps a deeper pool of resin, so cavities read darker than the surrounding face even with a single mix. That contrast can be used deliberately, but it should be designed rather than discovered after demoulding.

Violet epoxy plaque with recessed lettering made with SEP-955
Violet epoxy plaque with recessed lettering made with SEP-955. Letter cavities hold deeper resin and therefore read darker than the surrounding surface.

Polishing changes perceived colour. A matte demoulded surface scatters light and looks lighter and flatter; sanding and polishing to a gloss deepen the shade and reveal the translucency at the edges. Judge colour only after the piece has been finished the way the customer will receive it.

Controlling colour in thick sections

Target effectDosage on Part ANotes
Light violet tint1–2 phrTranslucent in thin sections
Pastel violet2–4 phr plus whiteWhite sets opacity, not the violet
Medium violet3–5 phrTypical artware and table range
Deep violet5–8 phrCheck dispersion at the real thickness

phr is parts of paste per hundred parts of Part A by weight. Weighing on the resin side keeps the ratio stable when the hardener mix ratio changes between products, which matters when a workshop runs several resins on the same bench. Dispersion and batch comparison for larger runs are described in violet epoxy flooring, coatings and FRP composites.

Processing for clean violet casts

  1. Condition resin, hardener and paste to a controlled workshop temperature before mixing.
  2. Weigh the paste into the resin and disperse to a uniform colour before adding hardener.
  3. Mix slowly enough to limit air entrainment; violet shows bubbles clearly in a gloss surface.
  4. Vacuum de-gas, or use pressure casting where the mould and resin allow it.
  5. Pour in planned stages for thick sections and respect the resin's stated maximum depth.
  6. Demould only after the part has reached its final hardness, then finish and polish before colour approval.

Limits

Photographs of castings are appearance references. They are not colorimetric measurements, and shade varies with resin, hardener, thickness, mould finish, lighting and polishing. Aromatic epoxy yellows under UV regardless of pigment, so exterior pieces need a UV-stable topcoat and a test on the finished object. SEP-955 provides no flame retardancy and makes no food-contact or toy-safety claim by itself. Heavy-metal-free status and RoHS or EN 71 suitability must be verified on the final formulation and article. Deep pours are limited by the resin's exotherm behaviour, not by the pigment.

FAQ

How much SEP-955 should I use for a deep violet casting?

Use 5 to 8 phr on Part A for a deep shade, then check the result at the actual thickness. A 10 mm coaster and a 40 mm river section made from the same mix will not look identical.

Why does my casting look lighter at the edges?

Thin sections transmit more light, so translucent violet appears lighter there. This is normal for a pigment that is not fully hiding, and it can be reduced with more paste, white addition or a thinner-walled design.

Can I polish a SEP-955 casting?

Yes. The pigment is dispersed through the cured body, so sanding and polishing expose the same colour rather than removing a surface layer. Finish the piece before judging colour. Product page: SEP-955 Dioxazine Violet Epoxy Pigment Paste. Series overview: epoxy color pastes.

Have Questions About Our Products?

Our technical team is ready to help you find the right color solution for your application.