SEP-9673 Phthalocyanine Green in Outdoor Coatings and Composites
Use SEP-9673 Pigment Green 7 in outdoor epoxy coatings and FRP, with blue-shade colour, flocculation, weathering and complete-system testing guidance.
SEP-9673 is a solvent-free epoxy pigment paste containing 25% chlorinated copper phthalocyanine Pigment Green 7. It is designed for clean blue-shade green industrial and outdoor epoxy coatings and composite surfaces requiring grade 8 light fastness and excellent pigment weathering. The cover image is an AI-generated appearance illustration for SEP-9673. It is not an outdoor coating, weathering or exposure test report.
Direct answer: where does SEP-9673 fit?
| System | Colour function | Primary qualification |
|---|---|---|
| Outdoor industrial coatings | Durable green equipment and product finishes | Hiding, flocculation, gloss and adhesion |
| Architectural epoxy coatings | Blue-shade green architectural and identification finishes | Yellowing, chalking and gloss retention |
| FRP gel coats | Durable green composite surfaces | Wet-out, print-through and weathering |
| Green identification coatings | Safety, product-family or service-zone colour | Contrast, hiding and actual exposure |
1. Why Pigment Green 7 is selected
Pigment Green 7 gives a clean blue-shade green together with outstanding light fastness and weathering, heat and solvent resistance. SEP-9673 delivers it as a 25% dispersion in a DGEBA epoxy carrier. Corrosion control, wear performance and UV protection remain responsibilities of the whole coating design rather than of the colourant alone.
2. Starting addition levels
| Target | SEP-9673 on Part A | What to verify |
|---|---|---|
| Light or blue-green tint | 1–3 phr | Rub-up, floating and substrate influence |
| Medium green | 3–5 phr | Colour development, hiding and mixed viscosity |
| Deep or full green | 5–8 phr | Rheology, levelling, cure and final appearance |
3. Flocculation, floating and rub-up
Phthalocyanine green is prone to flocculation-tone drift once it enters a customer formula. If colour moves after storage, after high shear or when white is let down, the cause usually sits in dispersion stability rather than in the pigment load. Give the batch time to wet out and equilibrate. Read colour after moderate shear and again after any high-shear stage. For green-white systems, assess rub-up, flooding and floating on the real substrate.
4. Outdoor ageing and topcoat selection
The pigment is rated grade 8 for light fastness with excellent weathering, yet yellowing, chalking and gloss retention belong to the finished epoxy and topcoat build.
5. Thermal boundary
The 280 °C figure belongs to the cured film and cannot be read as a service ceiling for a coating or laminate.
6. Related application questions
Thickness, dosage and light transmission in decorative parts are covered in transparent green epoxy casting and artware. Solvent and chemical exposure testing is discussed in green epoxy for chemical and solvent exposure.
Frequently asked questions
What shade does SEP-9673 produce?
It produces a clean blue-shade green based on Pigment Green 7.
Can SEP-9673 be used outdoors?
Pigment weathering is excellent, but real outdoor service also depends on the epoxy, hardener and topcoat chosen.
Why can green epoxy change colour after white pigment is added?
Flocculation, pigment mobility and dispersion interactions can shift colour development. Check rub-up, floating, flooding and equilibration time. Product: SEP-9673 Phthalocyanine Green Epoxy Pigment Paste. Related pages: industrial coatings and composite materials.