RFNC-1004 High-Loading Carbon Black Paste for Printing Inks, Adhesives and Industrial Films
A 40% Pigment Black 7 paste for high-hiding screen, flexo and gravure inks, pressure-sensitive adhesives, markers and industrial films, with dosage and rheology guidance.
RFNC-1004 is a 40% Pigment Black 7, binder-resin-free pigment paste for high-hiding solvent-based screen, flexographic and gravure inks, pressure-sensitive adhesives, oil-based markers and industrial films. Its 200 nm reported particle size and fineness and thixotropic nano-dispersion form support controlled incorporation, while PMA/PGMEA leaves binder selection to the formulator. Beyond color, the product offers a manufacturer-reported 10^15 Ω surface-resistance datapoint at 40% paste addition in its tested system, making it relevant to experimental electronic inks and functional black coatings that require both hiding and high resistance.
High pigment content changes the formulation starting point
A 40% pigment paste differs from a low-concentration colorant in both handling and formulation balance. RFNC-1004 can reduce the amount of paste needed to reach a given pigment level in ordinary coloring work, but it can also be evaluated at high addition for specialized films. These are two different formulation strategies. The general TDS guide is 1-3% for light shades, 3-6% for medium shades and 6-10% for deep or full shades. At 1%, 3%, 6% and 10% paste addition, the arithmetic pigment contributions are 0.40%, 1.20%, 2.40% and 4.00%. The separate 40% high-loading evaluation supplies 16% pigment. Do not treat the high-loading datapoint as a universal recommended dosage.
Printing and functional-film application matrix
| Sector | Potential role | Critical evaluation |
|---|---|---|
| Solvent-based screen inks | High-hiding black graphics, electronic markings and masks | Mesh transfer, edge definition, drying, blocking, adhesion and required surface resistance |
| Flexographic labels and packaging | Black text, solids and functional markings | Viscosity, anilox and plate interaction, density, dot quality, rub and drying |
| Gravure and metal-decoration inks | Dense black graphics and continuous-tone development | Cell release, solvent balance, printability, adhesion and resistance |
| LED and display printing | Light-blocking masks and borders | Backlight hiding, resolution, film thickness and ageing |
| Electronic marking inks | Black identification where high surface resistance is desired | Defined surface-resistance test, adhesion, cleaning exposure and dielectric tests where required |
| Pressure-sensitive adhesives | Black masking, identification or light-control layers | Tack, peel, shear, bleed, optical hiding and converting behavior |
| Oil-based markers | Full-hiding black marking ink | Flow, nib performance, drying, bleed and storage |
| Epoxy flooring and aerosol paints | Black coloration of compatible systems | Settling, spray or flow, cure, hiding, wear and chemical resistance |
| Industrial and protective coatings | High-hiding black finishes | Compatibility, film build, adhesion, weathering and chemical exposure |
Screen, flexo and gravure trials must use the real process
RFNC-1004 supplies dispersed pigment, not a finished ink. Confirm compatibility with the selected resin, solvent blend and additives. Check pigment shock, flocculation, viscosity drift and settling before printing. Then use the actual mesh, anilox, plate or gravure cylinder to evaluate transfer and drying. For screen inks, inspect edge definition, pinholes, mesh marks and blocking. For flexography, record anilox volume, viscosity, print density, dot gain and rub resistance. For gravure, examine cell release, solvent evaporation and continuous-tone quality. For LED or electronic printing, measure hiding and surface resistance on the same printed specimen rather than on an unrelated drawdown.
Adhesives and markers require functional controls
In a pressure-sensitive adhesive, compare colored and uncolored controls for tack, peel, shear, cohesion and aged adhesion. Check bleed, substrate staining, die-cutting and converting behavior. If the black adhesive is intended to block light, measure hiding at the final coat weight. If it is used near electronics, measure electrical behavior under the required conditions rather than assuming it from the paste datasheet. For oil-based markers, test capillary flow, nib wear, drying, bleed and long-term storage. Lightfastness 7-8 is a typical pigment property; final writing durability still depends on resin, solvent, substrate and exposure.
How to manage high-loading rheology and film properties
At high addition, the paste contributes pigment, dispersant and PMA/PGMEA as well as non-volatile material. The formulator must rebalance solvent, binder and additives rather than simply increasing colorant. Check viscosity over the relevant shear range, thixotropic recovery, leveling and storage stability. Prepare a dosage ladder instead of one extreme sample. Record hiding, gloss, adhesion, hardness, flexibility, cure and surface resistance at each level. A formulation with excellent hiding but poor leveling or adhesion is not a successful high-loading film. Likewise, a high initial resistance reading does not establish performance after humidity or thermal ageing.
Frequently asked questions
Is RFNC-1004 only for electronic inks?
No. It can be evaluated in conventional solvent-based printing inks, adhesives, markers and industrial coatings as well as functional electronic applications.
Does 40% pigment content mean every ink should contain 40% paste?
No. Pigment content and paste dosage are different. Ordinary coloring follows the TDS guide; 40% paste addition is a separate high-loading evaluation.
Can RFNC-1004 be used in food-packaging inks without further review?
No food-contact approval is supplied. The complete ink, substrate, print side, migration limits and target-market regulations must be assessed separately.
Does high hiding prove high surface resistance?
No. They are separate properties. Measure both on the actual printed or coated film.
Is the paste a ready-to-print ink?
No. It is a pigment dispersion that requires a compatible binder, solvent balance and application-specific additives. For ink, adhesive or industrial-film evaluation, provide the binder, substrate, process, target addition, film thickness and required hiding or electrical performance. Contact jia@henvastness.com. Product page: RFNC-1004 Resin-Free Insulating Black Nano Pigment Paste. Series: RFNC resin-free color pastes. Application pages: inks: flexo, gravure and UV, adhesives and 3C PSA and industrial coatings. Related articles: insulating carbon black for electrical coatings and full-hiding black for LED and optical films.